Hi,

Is it what you are looking for?

https://yade-dem.org/doc/yade.wrapper.html?highlight=triaxial#yade.wrapper.CapillaryTriaxialTest.autoCompressionActivation

Bruno


> I would like to ask, if it is possible to use Capillary Triaxial test
> preprocessor without applying deviatoric stresses. I just tried to
> assign all 'wall activated = 1' but I still have a heavy increase in the
> sigma1 values comparing to sigma3 ones.
>
> Best regards,
> Latifa El Ghezal


-- 